BDB
Absent Minded Professor
- Joined
- Aug 22, 2015
- Messages
- 2,556
- Reaction score
- 938
I'm building the modular fin can for my Binder Design Terrordactyl. I decided to use Titebond II because its strong, light, cheap and no one will see it once it's inserted into the airframe.
I applied the first set of fillets (~3/8" wide) nearly 24 hrs ago and let them sit at room temp. Since then they have dried somewhat, but they're still gooey. At this rate they won't be completely dry for 2-3 days. Is something screwed up?
I applied the first set of fillets (~3/8" wide) nearly 24 hrs ago and let them sit at room temp. Since then they have dried somewhat, but they're still gooey. At this rate they won't be completely dry for 2-3 days. Is something screwed up?