rfjustin
Well-Known Member
About a decade ago, I built a large curing oven to accommodate long tubes and completed boosters up to 60+” long. Original intent was to make my own carbon tubes eventually, but that never happened. @ECayemberg was kind enough to take said coffin off my hands a number of years ago in advance of a job change/move. That original build was mainly used for post curing fin cans with tip-to-tip laminations using Aeropoxy PR2032 resin and PH3660 hardener. Room temperature cure leaves Aeropoxy laminating epoxy noticeably tacky to the touch, but once post cured to about 190-200 degrees F, it’s very dry and hard.
I wanted to make a much smaller version today, mainly to bake fin cans only.
Here are some pics and links to products used on the build.
https://www.aircraftspruce.com/catalog/pnpages/01-42135.phphttps://www.homedepot.com/p/Woodgra...-x-36-in-Pine-Square-Dowel-10001818/206016659https://www.homedepot.com/p/Project...VFP3jBx1OHQ5FEAQYBCABEgLlavD_BwE&gclsrc=aw.ds
I wanted to make a much smaller version today, mainly to bake fin cans only.
Here are some pics and links to products used on the build.
https://www.aircraftspruce.com/catalog/pnpages/01-42135.phphttps://www.homedepot.com/p/Woodgra...-x-36-in-Pine-Square-Dowel-10001818/206016659https://www.homedepot.com/p/Project...VFP3jBx1OHQ5FEAQYBCABEgLlavD_BwE&gclsrc=aw.ds