- Joined
- Jan 30, 2016
- Messages
- 8,997
- Reaction score
- 3,525
Well shoot, I had a much better write-up for a theoretical TtT over FG-fin through FG-BT to FG-MMT, but clumsy me closed the draft tab.
In short: have you better recommendations for a more ridiculously over-strong system than PTM&W ( blenders of Aeropoxy )?
My thoughts:
Should ( maybe? ) give a minimum Tg of about 300F ... what have I completely missed / failed to understand / gotten exactly backwards?
In short: have you better recommendations for a more ridiculously over-strong system than PTM&W ( blenders of Aeropoxy )?
My thoughts:
- Bead blast fillet area, cut fin slots, clean with acetone
- ES6296 glue fin roots through wall into dams, wait an hour
- PT2846 tie layer
- HT2C fillets
- PT2846 glass laminate x 2-4 layers
- peel ply + breather + bag + vacuum, wait a day
- strip, trim as necessary
- PT1995 surface coat x 2, wait an hour
- 4 hours at each of 150 , 250, 350
Should ( maybe? ) give a minimum Tg of about 300F ... what have I completely missed / failed to understand / gotten exactly backwards?