I’m working on some Atlas parts. Ender 5, Amazonbasics white PLA. The Amazonbasics has taken some experimentation to get the first layer to go down nicely, but I think I have it dialed in. 210C first layer nozzle/ 70C first layer bed, dropping to 200/60.
I’m seeing a lot of shrinkage at the bottom. So bad it interferes with adhesion and the piece breaks loose about 75% up.
I tried a raft, instead of a brim, and the shrinkage is even worse. Thoughts? I thought bed too hot made for slumping, not shrinkage.
I’m seeing a lot of shrinkage at the bottom. So bad it interferes with adhesion and the piece breaks loose about 75% up.
I tried a raft, instead of a brim, and the shrinkage is even worse. Thoughts? I thought bed too hot made for slumping, not shrinkage.