I was cleaning out my workshop and found this, the first fincan from my PWF project.
A few layers of T2T and an epoxy coat or two and It'll be as good a new.
1/8in Quazisotropic CF fins from Dragonplate, Tube is 5 wraps of 3K carbon. Made with Aeropoxy. 1in Proline 4500 fillets. Peel Ply texture on the fin-tube area, ready for T2T or epoxy coating. It's a bit of a fix-er-uper.
Asking $50+shipping. I'll also be willing to trade for altimeters, EX supplies (liners, casting tubes, chems), or 38mm snap ring cases w/FCs and Nozzles.
I'll charge you actual shipping after it's shipped so I don't overcharge. I don't think It'll be too much more then $15, but it could be less.
Alex
A few layers of T2T and an epoxy coat or two and It'll be as good a new.
1/8in Quazisotropic CF fins from Dragonplate, Tube is 5 wraps of 3K carbon. Made with Aeropoxy. 1in Proline 4500 fillets. Peel Ply texture on the fin-tube area, ready for T2T or epoxy coating. It's a bit of a fix-er-uper.
Asking $50+shipping. I'll also be willing to trade for altimeters, EX supplies (liners, casting tubes, chems), or 38mm snap ring cases w/FCs and Nozzles.
I'll charge you actual shipping after it's shipped so I don't overcharge. I don't think It'll be too much more then $15, but it could be less.
Alex